Cauchy Layer
![](images/VSAEEllipsometer80.jpg)
![](images/VSAEEllipsometer81_001.jpg)
![](images/VSAEEllipsometer82.jpg)
![](images/VSAEEllipsometer83.jpg)
- Opt. Const. Fit boxes: work similarly to those of standard tabulated layers.
- The difference is that when neither box is checked, the optical constants are calculated using the Cauchy and exponential absorption functions.
- When either one box or both boxes are checked, the optical constants are taken from an internally stored list of fitting optical constants.
- This internal list is started with the functional values the first time a fit is performed.
- However, after the first fit of the optical constants, this internal list may be different from the functional values.